I never had a problem with cooling rate all the way up to 42mm package. I
have experienced warping on a smaller 'glob top' due to the fast heating
ramp of vapor phase. I now only use a convection oven with a 1 - 2 C/sec
heat ramp.
Jim Kittel
> -----Original Message-----
> From: Craig Hillman [SMTP:[log in to unmask]]
> Sent: Thursday, August 05, 1999 4:00 AM
> To: [log in to unmask]
> Subject: [TN] Large BGA's
>
> Hello Technetters,
>
> Standard vapor phase reflow profiles suggest cooling rates of
> between 1-4 degrees C/sec. Has anyone found it necessary to
> drastically reduce the cooling rate, down to C/minute, for large
> BGA's (45mm x 45mm)?
>
> Thanks in advance,
> Craig
>
>
> Dr. Craig Hillman
> CALCE Electronic Products and Systems Consortium
> University of Maryland
> College Park, MD 20742
> (301)-405-5316
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|