TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 26 Jan 2005 15:12:51 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Matthew Lamkin <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Matthew Lamkin <[log in to unmask]>
Parts/Attachments:
text/plain (175 lines)
Hmm, until Steve said so I wasn't.
perhaps it was just that no-one posted? :)

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Chris Ball
Sent: Wednesday, January 26, 2005 3:11 PM
To: [log in to unmask]
Subject: Re: [TN] Timely delivery of Technet posts...


....as am I.




                       "Blomberg, Rainer (FL51)"
                       <rainer.blomberg@HONEYWELL        To:   [log in to unmask]
                       .COM>                             cc:
                       Sent by: TechNet                  Subject:    Re: [TN] Timely delivery of Technet
                       <[log in to unmask]>                   posts...

                       01/26/2005 10:05 AM
                       Please respond to TechNet
                       E-Mail Forum; Please
                       respond to "Blomberg,
                       Rainer (FL51)"







I'm getting posts constantly throughout the day.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Matthew Lamkin
Sent: Wednesday, January 26, 2005 9:01 AM
To: [log in to unmask]
Subject: Re: [TN] Timely delivery of Technet posts...

Although only just turning mail back on, I too had this delay for the past
couple & I'm nothing to do with AOL ?

AOl - eeergh....spit!.. ;)

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Gary Ferrari
Sent: Wednesday, January 26, 2005 2:00 PM
To: [log in to unmask]
Subject: Re: [TN] Timely delivery of Technet posts...


Steve,

I also experience this problem. However, I think it may have something to
do with AOL. It would be interesting if we could obtain some sort of
indication as to what service providers are associated with the delayed
transmissions.

Regards,

Gary Ferrari


In a message dated 1/25/2005 8:34:08 PM Eastern Standard Time,
[log in to unmask] writes:

Hi  all!

I know I'm not the only one that receives Technet posts only a  couple of
times per day.

Once maybe early in the morning, and then  once again late in the evening
(around 8:00 pm central time). I'm curious  why this is happening. It has
never happened before...

We used to  get our posts through-out the day, real-time, as they were
posted, but no  more.

I've copied Keach on this post, hoping that he can explain things  for
us...

Am I the one of the few that experience this? What does  everybody else
experience?

-Steve  Gregory-

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe,  send a message to [log in to unmask] with following text in the
BODY (NOT the  subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery  of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To  receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information,  or contact Keach Sasamori at [log in to unmask] or
847-615-7100  ext.2815
-----------------------------------------------------





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



"This e-mail message is intended only for the use of the intended
recipient(s).
The information contained therein may be confidential or privileged, and
its disclosure or reproduction is strictly prohibited.
If you are not the intended recipient, please return it immediately to its
sender at the above address and destroy it."

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2