TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Technet (E-mail)" <[log in to unmask]>, "DesignerCouncil (E-mail)" <[log in to unmask]>
Date:
Mon, 24 Jan 2005 11:43:54 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Matthew Lamkin <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Matthew Lamkin <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
I have just noticed the barrels on some boards that we now get silver plated instead of tin plated so as to be lead free.

I can clearly see the laminate strands through this hole and many others on the boards.

What difference is this from an ordinary tin plated hole?
looking at older boards, I can see nice shiny & flat holes & no ridges.

Is there something wrong with the holes that have been silver plated or would they look like this anyway?

What impact does this have on the current carrying ability of a plated hole?

I have managed to get a picture taken of one hole to indicate what I'm on about.

http://www.ukxboxgamers.co.uk/BARRELL.jpg

Thankyou,
Matthew Lamkin.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2