TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 7 Jul 2006 15:58:08 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Carl Beharry <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Carl Beharry <[log in to unmask]>
Parts/Attachments:
text/plain (37 lines)
Hello fellow Technetters,

Would like some advise from the experts out there.

We have always assembled pcb with minimal solder balls that usually gets 
washed away in the cleaning process, hence not creating any major problems.
However, recently we have been getting involve with more complex boards that  
has alot of 1mm and .8mm low profile bga's.
The problem that we are noticing is that the solder balls that never was a 
problem before are now getting stuck under the bga's, sometimes creating shorts. 
I am not sure if we can eliminate solder balls completely but would 
like to know how the experts are resolving a problem of this sort.

Thanks in advance for your input.
Regards,
Carl Beharry 
Ectronics, Inc.
855 Industrial Hwy
Cinnaminson, NJ 08077
Phone : (856) 829-7161
Fax : (856) 829-6950
Email : [log in to unmask]
  




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2