TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Wed, 9 Dec 2009 16:22:46 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
Fabricators,

This is an opportunity to influence the acceptability of your product!

The IPC Standards Development Committee is working on the next
revision to IPC-A-600 (Acceptability of Printed Boards) which is a
visual reference companion to IPC-6012.

One of the items we are currently discussing is the acceptability of
haloing along the board edge. Here is a link to where we stand now:

http://frontdoor.biz/PCBportal/IPC-A-600H213.jpg

The problem is, if the designer violates the recommendation in the
current IPC-2221 design guideline and puts traces or planes too close
to the board outline, with the current wording of "whichever is less"
your boards can be considered rejectable with even a very small
amount of haloing. Even intentional features like edge fingers can
make your boards rejectable.

We aren't sure if we should reword this (and if so, how?)

So the ball is in your court (because unless there is a logical consensus
we probably won't change it).
I'll compile and submit any responses to the next committee meeting.

Jack (aka "the new guy")

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2