I do not suggest a high temperature baking, but I've heard of some
people baking to Tg temperature or higher. It is bad for the board,
I just wanted to point it out.
Alain Savard, B.Sc.
Chemical Process Analyst
CAE Electronics Ltd.
e-mail: [log in to unmask]
-----Original Message-----
From: Howieson, Rick [mailto:[log in to unmask]]
The purpose of baking is to remove moisture. I don't think you need to
bake at the glass transition of the laminate. I have mentioned common
sense in the TrainerNET forum and it certainly can be applied in this
forum.
Bueno, Bye
Rick Howieson
>-----Original Message-----
>From: Alain Savard [SMTP:[log in to unmask]]
>It increases cross linking inside the epoxy of the laminate,
>making is slightly more brittle and harder every time you
>bake it. It alsoi ncreases the speed of tin oxide formation,
>in effect it ages the board.
>
>It has also been suggested that a high temperature bake
>(> Tg) may cause warpage in a pressed board.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|