TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Alain Savard <[log in to unmask]>
Date:
Tue, 26 Oct 1999 12:33:06 -0400
MIME-Version:
1.0
X-To:
"Howieson, Rick" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Alain Savard <[log in to unmask]>
Parts/Attachments:
text/plain (44 lines)
I do not suggest a high temperature baking, but I've heard of some
people baking to Tg temperature or higher. It is bad for the board,
I just wanted to point it out.

Alain Savard, B.Sc.
Chemical Process Analyst
CAE Electronics Ltd.
e-mail: [log in to unmask]

-----Original Message-----
From: Howieson, Rick [mailto:[log in to unmask]]

The purpose of baking is to remove moisture. I don't think you need to
bake at the glass transition of the laminate. I have mentioned common
sense in the TrainerNET forum and it certainly can be applied in this
forum.
Bueno, Bye
Rick Howieson

>-----Original Message-----
>From:  Alain Savard [SMTP:[log in to unmask]]

>It increases cross linking inside the epoxy of the laminate,
>making is slightly more brittle and harder every time you
>bake it. It alsoi ncreases the speed of tin oxide formation,
>in effect it ages the board.
>
>It has also been suggested that a high temperature bake
>(> Tg) may cause warpage in a pressed board.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2