     Yes, ripple is AC leakage into what should be a pure DC current and 
     can adversely affect plating if too high.  Ripple is measured by AC/DC 
     of the present setting and usually decreases as the rectifier is 
     turned up.  As a general rule, Max. AC ripple should not exceed 5%.
     
     DNHJR


______________________________ Reply Separator _________________________________
Subject: GEN: Rectifiers
Author:  [log in to unmask] at corp
Date:    12/20/96 6:13 AM


Is it true that rectifiers generate a constant minimum AC voltage (rms) 
that causes variable ripple depending on actual or overall voltage?  In 
explanation, is ripple defined by the minimum AC voltage over the rated 
output voltage only?
     
Could the group enlighten me on the subject of minimizing ripple and how 
it affects plating?  There's been much discussion about copper plating, 
and I would appreciate some information on this topic.
     
Chemist, IUP, CU  
     
P.G. Wilson
[log in to unmask]
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2