TECHNET Archives

July 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 17 Jul 2018 12:16:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Showers <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="utf-8"
Content-Transfer-Encoding:
quoted-printable
From:
Wayne Showers <[log in to unmask]>
Parts/Attachments:
text/plain (16 lines)
For most of my Urethane applications, I have used Kleen-Strip Lacquer thinner.  The best process is to apply, wait 5-10 minutes and brush with an ESD safe stiff bristle brush, repeat as necessary.  Use a 50% IPA/DI Water blend for final surface clean.  If water is an issue, use a 75% IPA/Water blend (this is the same blend in Ionograph columns).

Simple Air dry is also effective, just make sure you have lots of ventilation and/or a Class 'A' oven.

Best thing is that, for now, you can purchase Kleen-Strip in most hardware stores.

SDS:
CAS # Hazardous Components (Chemical Name)
3. COMPOSITION/INFORMATION ON INGREDIENTS Concentration
67-56-1 Methanol {Methyl alcohol; Carbinol; Wood alcohol}                           25.0 -35.0 %
67-64-1 Acetone {2-Propanone}                                                                  20.0 -30.0 %
NA Petroleum Hydrocarbon Mixture (Alkanes and Cycloalkanes)                      20.0 -30.0 %
141-78-6 Acetic acid, ethyl ester {Ethyl acetate}                                           <15.0 %
108-88-3 Toluene {Benzene, Methyl-; Toluol}                                               < 5.0 %
111-76-2 Ethanol, 2-Butoxy- {Ethylene glycol n-butyl ether, (a glycol ether)}  < 5.0 %