Hi All,
I was posed this question by one of our customers. I don't have any
experience with nickel plated wire, but it would seem to me to be difficult to solder
to. I've used tin plated, and silver plated wire before with no problems. But I
didn't know that silver plated wire had corrosion problems. Any inputs?
In the future we are going to be changing to specify a nickel plated wire
(M22759/10-28-9) for PWA repair. The previous part number was a silver plated
wire. We haven't used this before. Do you or any of your manufacturing people
know of issues with solderabiliby when using a nickel plated wire or any
special process that should be used?
The history of this is IPC-7721 paragraph 6.1 says silver plated wire must
not be used because it can cause corrosion of wire in certain situations. Turns
out that when you follow MIL-23200 the allowed wire is either silver plated or
nickel plated. We would have preferred tin plated wire but it doesn't appear
to fall under the allowed MIL-23200 options.
Thanks in advance!!!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|