AMP published a paper on this thin-gold topic for 'AMP Engineers Week'
in 1997, called 'A Perspective On The Characteristics Of Thin Gold
Platings'. It's part of a larger bound publication and should be
available from AMP. I suggest you call Bob Kuhn at 717-986-3631, who
manages the Technical Information Center. He/they should be able to
help.
> -----Original Message-----
> From: Carlos R. Robert [SMTP:[log in to unmask]]
> Sent: Friday, February 06, 1998 2:30 PM
> To: [log in to unmask]
> Subject: [TN] Gold for edge-board connectors thickness
>
> Hello,
>
> Although IPC-6012 specifies a minimum thickness of 0.8
> micrometers (30
> micro inches) of gold for Class 1 and 2 edge-board connectors,
> it seems
> that more and more suppliers are suggesting thinner and thinner
> gold
> plating as a low cost alternative.
>
> Looking back into this forum's archives, I found the 1995 tread
> 'Where
> did 30m" for gold Tab plating come from?' with very good
> information
> but no definite answer. One poster performed an experiment
> about
> thickness and connection cycles (see attached message fragment),
> and
> found out that a 20m" finger gave up at about 10 cycles. If
> these
> results are still valid (I don't see why not), how come PCB
> vendors are
> even suggesting flash gold (2 to 7 micro inches) as an
> acceptable
> option?
>
> I also posed this question (via E-mail) to two connector
> manufacturers,
> AMP and Burndy. AMP answered immediately but did not provide a
> definite
> thickness (I got their connector's specs and insertion rates
> thought).
> I have not received a reply from Burndy yet.
>
> Do anyone has more information or pointers about this issue?
> Has
> technology advanced so much that thin flash gold is acceptable
> for
> edge-board connectors in a Class 1 product?
>
> Thanks,
>
>
> Carlos R. Robert
> Hewlett-Packard Puerto Rico
>
[Rhoads, Randall E] <previous message deleted>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|