TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"Rhoads, Randall E" <[log in to unmask]>
Date:
Wed, 11 Feb 1998 11:51:08 -0500
Content-Type:
text/plain
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Rhoads, Randall E" <[log in to unmask]>
Parts/Attachments:
text/plain (79 lines)
While I'm not very familiar with this subject, I forwarded it to someone
in AMP who is - and this was his reply.

> -----Original Message-----
> From: Bock, Ed M
> Sent: Wednesday, February 11, 1998 11:04 AM
> To:   Rhoads, Randall E
> Subject:      RE: [TN] (Fwd) Gold Plated Edge Connectors
>
> Randy:
>
> If the board needs to re-mated, then the gold plating is not doing
> it's job.  Wiping action is of benefit in disrupting films and
> particulated contamination.  If upon initial mating the system
> performs - then why exercise the connection at a later date - unless
> the system is not immune to corrosion ingression into the interface -
> and re-mating could be a short time fix. A better solution would be to
> use a contact lube that has known anti-corrosion attributes : unmate -
> clean - lubricate - re-mate.
>
> Ed Bock
> Member of Technical Staff
> Interconnection Surface Science
> M.S. 106-13
> 717-986-7698     -5218(FAX)
>
> ----------
> From:         Rhoads, Randall E
> Sent:         Friday, February 06, 1998 7:55 AM
> To:   Bock, Ed M
> Subject:      FW: [TN] (Fwd) Gold Plated Edge Connectors
>
> -----Original Message-----
> From: John Parsons [SMTP:[log in to unmask]]
> Sent: Thursday, February 05, 1998 3:48 AM
> To:   [log in to unmask]
> Subject:      [TN] (Fwd) Gold Plated Edge Connectors
>
> Good Morning,
>
> The following query was received this morning.  While I can provide
> some real life experiences for
> this gentleman, I thought that this group could provide some more
> concrete information.
>
> Thanks
>
> John Parsons
> Circuit Graphics Ltd.
>
> Hi!
>  I am curious about corrosion and gold plated connectors.
>  I work in a sawmill - dusty enviroment.
>  There are PM's which call for unplugging boards and cleaning
>  these connectors, once a year.
>
>  My experience is Gold doesn't corrode.
>  Leave the boards for a longer time. Unplugging these boards,
>  in my opinion, would create more of a problem then cleaning
>  would prevent. (unplugging/plugging - starts to scrape off
>  the Gold plating.
>
>  What do you suggest.
>    Steve Redly,
>     Weyerhaeuser, Lumby.
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2