TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Macko, Joe @ IEC" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Macko, Joe @ IEC
Date:
Tue, 24 Jul 2007 10:13:25 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (46 lines)
Good morning All.

 

One of our CMs is experiencing either non-wetting and/or dewetting on
the end cap(s) of some 0402 capacitors provided by 2 different
manufacturers. One Cap manufacturer plates using Sn90Pb10 and the other
plates using SN95Pb5. The smt CM is using Kester Hydromark 531 WS,
Sn63Pb37 paste.  The profile is obviously a SnPb type profile.

 

Samples of each caps were sent to an outside lab for a solderability
test and both failed a Dip and Look Solderability test per J-STD-002B -
see attachments. However, both Cap providers informed us that their
samples passed their Dip and Look solderability test.

 

Question --  Subsequent smt runs using the same paste type and profile
but with "pure tin" plated capacitors showed no evidence of either
wetting or de-wetting, which begs the question, what is different about
these Caps that cause the wetting/dewetting issues. Plating?????

 

Look forward to anyone's comments, experience, etc...  People either
think it is capacitor issue or a smt process issue.   thanks

 

-Joe 

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2