Good morning All.
One of our CMs is experiencing either non-wetting and/or dewetting on
the end cap(s) of some 0402 capacitors provided by 2 different
manufacturers. One Cap manufacturer plates using Sn90Pb10 and the other
plates using SN95Pb5. The smt CM is using Kester Hydromark 531 WS,
Sn63Pb37 paste. The profile is obviously a SnPb type profile.
Samples of each caps were sent to an outside lab for a solderability
test and both failed a Dip and Look Solderability test per J-STD-002B -
see attachments. However, both Cap providers informed us that their
samples passed their Dip and Look solderability test.
Question -- Subsequent smt runs using the same paste type and profile
but with "pure tin" plated capacitors showed no evidence of either
wetting or de-wetting, which begs the question, what is different about
these Caps that cause the wetting/dewetting issues. Plating?????
Look forward to anyone's comments, experience, etc... People either
think it is capacitor issue or a smt process issue. thanks
-Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|