To add to Wayne's input, make sure you call out the right OSP depending on the board technology...not all OSP's are the same.
Steve
Sent from my BlackBerry 10 smartphone.
Original Message
From: Wayne Thayer
Sent: Friday, August 15, 2014 11:28 AM
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] surface finish for "bare" copper
OSP
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mark Larson
Sent: Friday, August 15, 2014 1:12 PM
To: [log in to unmask]
Subject: [TN] surface finish for "bare" copper
Hi,
I've got a board that needs bare copper, many years ago I had this as well and
seem to recall that they can put on some kind of finish in the process that
does not leave it bare, but does protect it in the processing of the board,
and consequently does offer some protection to the end user. Anybody know what
that is or how I call it out?
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|