TECHNET Archives

August 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Stadem, Richard D." <[log in to unmask]>
Date:
Wed, 6 Aug 2014 13:52:26 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>, Chris Mahanna <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (77 lines)
Hi Richard!

Done!

http://stevezeva.homestead.com/Soldermask_view.pdf

Steve


On Wed, Aug 6, 2014 at 1:40 PM, Stadem, Richard D. <
[log in to unmask]> wrote:

> I have taken the picture, blown it up, modified it to show the contrast a
> little better, and now it is easier to see where the soldermask makes
> contact almost at the beginning of the point where the crack starts on the
> left side. I am hoping Steve can post it. The rest of you will not see the
> attachment because Technet strips all attachments.
> During thermal cycling the masking is continually pushing against the
> solderball joint at the base near the edge of the pad. The pressure is both
> inward and upward. That is what causes the stress that leads to formation
> of the crack in the coarsened crystalline structure of the solder joint,
> and also what causes it to continue (the z-axis prying force upward). It is
> actually an extrusion process.
> At least that is what I think, based only on what I can see in the picture.
> dean
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
> Sent: Wednesday, August 06, 2014 1:49 PM
> To: [log in to unmask]
> Subject: [TN] SJ fracture signature
>
> We see hundreds of cracked solder joints every year, but I can't say that
> I've ever seen one quite like this.  I have some suspicions, but I'll keep
> them to myself, as to not prejudice the crowd.
> EDS maps are forthcoming.
>
> This is a caught in-the-wild field failure of a 48-pin BGA Reballed to
> SnPb ENIG on board side Ni barrier on component side
>
> http://stevezeva.homestead.com/45268-1.JPG
>
> http://stevezeva.homestead.com/45268-2.JPG
>
> http://stevezeva.homestead.com/45268-8.JPG
>
> Thoughts?  And Thanks to Steve!
>
>
> Chris Mahanna
> President, Technical Manager
> Robisan Laboratory Inc.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2