TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Hart, Dale L CTR USAF AFMC AFRL/RXSA" <[log in to unmask]>
Date:
Mon, 4 Oct 2010 11:44:14 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Phil Bavaro <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (92 lines)
Hi Dale,

Was this deflection seen during the print process?  Many times the
printer has better support than the placement equipment does (but not
necessarily).  The placement equipment should be putting down the
components into the paste.

If indeed the process was out of control and the paste thicknesses
varied to the extreme, then yes there is more solder possible.
Typically I have seen sag in larger panels due to weak routing but as
long as the paste deposition was well controlled, we did not see issues
after reflow.

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hart, Dale L CTR
USAF AFMC AFRL/RXSA
Sent: Monday, October 04, 2010 11:26 AM
To: [log in to unmask]
Subject: [TN] pick and place /board deflection

 

I was on the shop floor and noticed deflection in the 8x8 inch panel
that
was being populated.  Would the deflection in the middle of the panel
cause
components to sit higher on the paste and thus have a slightly higher
solder
joint height than components on boards along the rails?       Thanks in
advance

 

Dale L. Hart

Universal Technology Corporation (UTC)

Failure Analysis

1270 North Fairfield Road

Dayton, Ohio  45432-2600

(937) 656-9165

Fax (937) 656-4600

Email:  <mailto:[log in to unmask]> [log in to unmask]

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2