TECHNET Archives

June 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 26 Jun 2003 12:59:07 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Charles Caswell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Charles Caswell <[log in to unmask]>
Parts/Attachments:
text/plain (149 lines)
My first choice would have been to use the "mini-wave" but couldn't because of clearance. I heat the board in an oven to 250 degF. grab it with welding gloves and run to my soldering iron. Not the most precise process but it works. Fortunatly I don't have to do very many of them.

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, June 26, 2003 11:01 AM
To: [log in to unmask]; Charles Caswell
Cc: [log in to unmask]
Subject: Re: [TN] Fab shops that are UL certified to do 6-oz copper...



Hi Charles! We have a power supply assembly which is 0.90 thick and
contains 18 total ozs. of copper - that exceeds the limits of hand
soldering but we have been able to "mini-wave solder" it just fine. I can
just imagine that 12 layers of 4 oz. would be equally difficult. What
processes to you use to process a 12 layers of 4 oz.  assembly?

Dave


                                                                                                                                       
                      Charles Caswell                                                                                                  
                      <CharlesC@FESCORP        To:       [log in to unmask]                                                      
                      .COM>                    cc:                                                                                     
                      Sent by: TechNet         Subject:  Re: [TN] Fab shops that are UL certified to do 6-oz copper...                 
                      <TechNet@listserv                                                                                                
                      .ipc.org>                                                                                                        
                                                                                                                                       
                                                                                                                                       
                      06/26/2003 09:59                                                                                                 
                      AM                                                                                                               
                      Please respond to                                                                                                
                      "TechNet E-Mail                                                                                                  
                      Forum."; Please                                                                                                  
                      respond to                                                                                                       
                      Charles Caswell                                                                                                  
                                                                                                                                       
                                                                                                                                       




hOW ABOUT 12 LAYERS OF 4OZ COPPER. Hand solder.

-----Original Message-----
From: Dave Hillman [mailto:[log in to unmask]]
Sent: Thursday, June 26, 2003 9:39 AM
To: [log in to unmask]
Subject: Re: [TN] Fab shops that are UL certified to do 6-oz copper...


Ok Steve, I'll bite! What type of application utilizes 6 oz. copper layers?
I have visions of trying to solder to a "bar" of copper if the resulting
printed wiring board had 4-6 layers of 6 oz. copper!

Dave Hillman
Rockwell Collins
[log in to unmask]




                      Steve Gregory
                      <[log in to unmask]        To:
[log in to unmask]
                      M>                       cc:
                      Sent by: TechNet         Subject:  [TN] Fab shops
that are UL certified to do 6-oz copper...
                      <TechNet@listserv
                      .ipc.org>


                      06/26/2003 09:14
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      SteveZeva






Mornin' all!

Anybody know of any Fab shops that are UL certified
to do 6-oz copper? We work with some that are certified
to do 5-oz, but not 6-oz.

One of our customers is requesting this from us...

Thanks!!

-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2