TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Fogelqvist Peter <[log in to unmask]>
Reply To:
Date:
Mon, 27 Apr 1998 08:34:35 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
HIHAT44 wrote:
>
> Hello all,
>      I've been working on a simple, cost effective way of treating electroless
> nickel.  So far the batch treatment of this spent bath is one of the more
> difficult ones I have to deal with.  There are alot more electroless nickel
> baths running out there and my customers requests to help them treat the spent
> baths are becoming more frequent.  So far I've had pretty good results but I
> would like to know if anyone out there has this process dialed in yet?
>
> Steve Wentz
> Florida CirTech
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
Hi Steve
I know about one method. Adjust pH to 8.8(with NaoH) and
electrolytically
plate the nickel using large area cathodes.
Pete

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2