HIHAT44 wrote:
>
> Hello all,
> I've been working on a simple, cost effective way of treating electroless
> nickel. So far the batch treatment of this spent bath is one of the more
> difficult ones I have to deal with. There are alot more electroless nickel
> baths running out there and my customers requests to help them treat the spent
> baths are becoming more frequent. So far I've had pretty good results but I
> would like to know if anyone out there has this process dialed in yet?
>
> Steve Wentz
> Florida CirTech
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
Hi Steve
I know about one method. Adjust pH to 8.8(with NaoH) and
electrolytically
plate the nickel using large area cathodes.
Pete
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|