Hi Alan,
I have not had any issue with ENIG. I am sure it is harder, but I feel
the whole press-fit process is more dependant on the finished hole
diameter.
Please follow the recommended finshed hole diameter.
Work with your fab vendor to insure they can manufature the fab to the
finished hole tolerances required.
Work with your fab vendor to insure they can manufature the fab to the
recommended pre-drill.
Insure you are geting at least .001" of plating in the barrel.
Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
825 University Avenue
Norwood, MA 02062-2643
(T) 781-467-5468
(C) 508-631-1832
(F) 781-461-0993
Alan Kreplick <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/17/2007 06:44 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Alan Kreplick <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] PWB-Hole Plating for Press-Fit Connectors
To All:
Anyone want to share thoughts/comments/guidelines on pwb-hole plating
press-fit connectors. Specifically ENIG vs. Tin/Lead.
I've been told and saw in one article that tin/lead (soft) is preferred
over ENIG (nickel hard).
Thanks in advance,
Al Kreplick
Sr. Manufacturing Engineer
Circuit Card Assembly
Air-toAir/Precision Strike/Land Combat
Raytheon Integrated Defense Systems
978-470-9931office
978-245-1702 pager
978-470-4307 fax
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|