It's very difficult to answer your question as all surface finishes suffer
with solderability issues based on the control of the original fabrication
process or what assembly engineers like me to do to the poor green boards.
It may be better to be a little more specific on the question to help
TechNet answer your question, the solderability experts out there could
write war and peace on the question posed.
If it helps lets sit down at the seminar in Istanbul on 22nd October at the
ESMAN Seminar
You should also read through the IPC document IPC 4552 the IPC agent in
Turkey is also ESMAN.
Many thanks and all the best
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
www.SolderingStandards.com
PCB Design for Manufacture & Assembly Workshop 15th October
www.ASKbobwillis.com
PCB Inspection & Quality Control Workshop 3rd November
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 4th November
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Halil Ibrahim YASLAK
Sent: 14 August 2009 06:22
To: [log in to unmask]
Subject: [TN] Solderability of ENIG
Hello everybody,
Does ENIG ( Electroless Nickel Immersion Gold) finish for printed circuit
board cause any solderability problem? Is there anyone who has faced a
soldering problem because of ENIG?
Thank you in advance for your help.
Saygılarımla / Best Regards,
Halil İbrahim YAŞLAK
ASELSAN Inc. MGEO Division
P.O.Box:30, Etlik 06011- ANKARA / TURKEY
Phone:(90-312) 847 5300 / 4907
Fax: (90-312) 847 5320
######################################################################
Dikkat:
Bu elektronik posta mesaji kisisel ve ozeldir. Eger size
gonderilmediyse lutfen gondericiyi bilgilendirip mesaji siliniz.
Firmamiza gelen ve giden mesajlar virus taramasindan gecirilmekte,
guvenlik nedeni ile kontrol edilerek saklanmaktadir. Mesajdaki
gorusler ve bakis acisi gondericiye ait olup Aselsan A.S. resmi
gorusu olmak zorunda degildir.
######################################################################
Attention:
This e-mail message is privileged and confidential. If you are
not the intended recipient please delete the message and notify
the sender. E-mails to and from the company are monitored for
operational reasons and in accordance with lawful business practices.
Any views or opinions presented are solely those of the author and
do not necessarily represent the views of the company.
######################################################################
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|