TECHNET Archives

August 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Date:
Thu, 27 Aug 2009 18:32:45 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Willis <[log in to unmask]>
Subject:
From:
Bob Willis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<008601ca272e$0b939280$22bab780$@com>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (175 lines)
All good stuff buy the oil test is cheaper to do than a section, with care
its also no destructive. Also after documenting the fault you can also test
the actual hole or adjacent via in pad causing the problem.

Many thanks
 

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
www.SolderingStandards.com 


New Package on Package Workshops 24th November
www.ASKbobwillis.com/PoPWorkshops.pdf 
PCB Design for Manufacture & Assembly Workshop 15th October
www.ASKbobwillis.com 
PCB Inspection & Quality Control Workshop 3rd November
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 4th November
www.ASKbobwillis.com/faworkshops.pdf

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: 27 August 2009 16:50
To: [log in to unmask]
Subject: Re: [TN] Via-in-pad blowing bubbles

Makes sense to me. If the x sections look good for thickness and the hole
drill is good you are probably right about the board outgassing.
The mask we use to hand plug vias is heat cured. A good 2 hr bake and we
don't have problems. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Thursday, August 27, 2009 10:47 AM
To: [log in to unmask]
Subject: Re: [TN] Via-in-pad blowing bubbles

Bob et al,
Sorry we don't have blinds outgassing.  If we see some I'll send a sample to
you. Obviously I forgot to mention the via type.  They are through vias with
single sided solder mask plug.  The plug is very deep (>75%), and maybe a
separate mask process.  Different mask?  I doubt that the board is
outgassing through the via because we've got ~1.8 mil of uniform plating.
How about incomplete plug cure?  I think that I may have some evidence of
that.

Chris

-----Original Message-----
From: Bob Willis [mailto:[log in to unmask]] 
Sent: Thursday, August 27, 2009 7:23 AM
To: 'TechNet E-Mail Forum'; Chris Mahanna
Subject: RE: [TN] Via-in-pad blowing bubbles

If you have via in a pad and its solder coated or reflowed with paste what
you describe can happen. If there is still volatile material either in the
hole, a void below the level of the solder or thin copper plating outgassing
through the copper plating can happen. Not however on gold over nickel
boards. The eruption and outgassing will be random depending on what is
there, speed of heating and how long the solder remains molten.

Just like any gassing from a plated through hole you can see a nice ball, a
balloon blow out or a sunken joint and this can be all associated with
outgassing. The classic problem with through vias is when engineers try to
fill small vias on side one reflow, then spend hours cleaning balloons off
side two before printing again.

If you simply find a sample board with the problem you describe and place it
under a microscope, fill the view with a group of pads in question. Take a
micro soldering iron and touch sample pads and wash what happens. You can
use the old oil outgassing test I have used for years to see the outgassing
from the vias on a bare board Unfortunately I don't have a via example to
show you but if you look at http://defectsdatabase.npl.co.uk and do a search
for via outgassing you will see some a video and gif animation and images.

If someone has some good examples of blind vias that are outgassing, send me
a board and I will test it and share the video on TechNet. I have tested
vias in the is way before for customers but never videoed the results.

Many thanks

Many thanks
 
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
www.SolderingStandards.com 


New Package on Package Workshops 24th November
www.ASKbobwillis.com/PoPWorkshops.pdf
PCB Design for Manufacture & Assembly Workshop 15th October
www.ASKbobwillis.com PCB Inspection & Quality Control Workshop 3rd November
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 4th November
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: 27 August 2009 02:34
To: [log in to unmask]
Subject: [TN] Via-in-pad blowing bubbles

Hello netters-

Have we a term for vias-in-pad blowing solder ball bubbles to the point of
bridging?
Regardless, is there a unique cure for the problem?
I wonder because- how does one get just enough pressure to blow the large
bubble, but not blow-out?   Bad luck?
Or is it not that unusual, and just usually gets screened before it gets to
me?

Chris


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2