I recently ran a few test assemblies (with immersion Ag finish, of course)
through thermal cycling (for 2nd level reliability).  At the end of the
test, some of the non-soldered metal area (EMI contact) got the yellow
tarnish.  When probed with a multimeter I measured significant increase in
contact resistance.

I read a lot of comments on the presence of sulfur and chlorine (or their
ionic counterparts) as being the possible root cause.  My question is: what
is the chemical reaction(s) here?  Are those agents attacking the Ag or the
organic co-deposited with the Ag?  Does anybody know what the yellow stuff
is?

Mason Hu

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2