Hi Roger! One of the issues with solder creep data is that you need to
understand as completely as possible the conditions of the testing that
generated the data. There is lots of solder creep data in the public
domain but you need to use it cautiously. One source of solder mechanical
property data that I have found useful in the "Solder Alloy Data" ,
International Tin Research Institute Publication #656. The test protocol
for that data set is reasonably documented and reviewable. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Roger Mack <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04/14/2010 09:23 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] solder creep charts
Does anyone have a detailed solder creep graph (shear stress N/mm˛ vs.
time to rupture) for tin lead solder?
I have been using Figure 4.35 from Klein Wassink's Soldering in
Electronics. This graph starts at a shear stress of 1.
We have run a ProE computer model that shows a shear stress value of
0.6N/mm˛ on the connector pins of two boards that are mounted together. We
have placed some samples to bake at the maximum service condition
temperature to validate the computer model is realistic. It does not take
much of an extrapolation error on a small text book graph to be off by an
order of magnitude.
Roger Mack P.Eng.
Manufacturing Specialist
Parker Hannifin Electronic Controls
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB R3T 1T4 Canada
direct 204 453 3339 x373
[log in to unmask]
www.parker.com/ecd
PLEASE NOTE: The preceding information may be confidential or
privileged. It only should be used or disseminated for the purpose
of conducting business with Parker. If you are not an intended
recipient, please notify the sender by replying to this message and
then delete the information from your system. Thank you for your
cooperation.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|