TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joe Fjelstad <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 17 Apr 2007 12:33:48 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (40 lines)
 
In a message dated 4/17/2007 8:33:13 AM Pacific Daylight Time,  
[log in to unmask] writes:

The  improved reliability should not have come as a surprise. Consider what 
is  
happening: 
(1) the solder balls are at their full diameter when BGA is  placed,
(2) the epoxy fixes the distance between PCB and BGA at that  diameter value,
(3) during reflow, the epoxy expands opening the solder gap  further,
(4) on cooling, that solder balls are prevented by the epoxy from  collapsing,
(5) you have the equivalent reliability of using non-melting  10Sn90 Pb 
solder 
balls,
and (6) this results in the reliability  improvement observed.
I have been pushing this for   ceramic  chipp components for some time.





Very crisp summary, Werner. Thanks
 
All the best, 
Joe 



************************************** See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2