TECHNET Archives

July 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Linda Woody <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 25 Jul 2002 07:48:52 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Hi Technet,
I currently have a solder anamoly I need to understand. The component in
question is a very large ceramic leaded (glass bead seals on leads)device
with leads on two sides only. The leads are gold and have been pretinned.
After reflow the solder joints look great (so I believe the thermal profile
is good). The problem is seen after a vacuum thermal bond to a heatsink.
The temperature is 250 degrees F. for 5 hrs. at 26 inches of mercury. Also
the component is being stacked to the PWB (polyimide material) using a bead
of Hysol 151 epoxy on both ends.

Post bond the solder joints look disturbed and oxidized. I understand the
oxidation and am not concerned over this. The disturbed look concerns me.
Is this due to a CTE mismatch? Could there be some other explaination? The
joints aren't fractured but the lead foot appears to have shifted in the
solder. Any theories or possible explainations would be greatly appreciated.

Thanks all,

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2