Hi Technet, I currently have a solder anamoly I need to understand. The component in question is a very large ceramic leaded (glass bead seals on leads)device with leads on two sides only. The leads are gold and have been pretinned. After reflow the solder joints look great (so I believe the thermal profile is good). The problem is seen after a vacuum thermal bond to a heatsink. The temperature is 250 degrees F. for 5 hrs. at 26 inches of mercury. Also the component is being stacked to the PWB (polyimide material) using a bead of Hysol 151 epoxy on both ends. Post bond the solder joints look disturbed and oxidized. I understand the oxidation and am not concerned over this. The disturbed look concerns me. Is this due to a CTE mismatch? Could there be some other explaination? The joints aren't fractured but the lead foot appears to have shifted in the solder. Any theories or possible explainations would be greatly appreciated. Thanks all, --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------