In repsonse to your request you made on technet for a High Temp PCB we may
have an answer for you !
Please vist our Web Site: www.thermalworks.com
We have several products one is or Tg747 ( Glass Transition Temperature of
747 degree F )
We also have a product line of what we call STABLCOR, which is a Thermally
managed, closely matched CTE PCB technology with thermal transfers up to
1000 W / m K.
Mark A. Roslawski
Vice President Marketing
ThermalWorks
2910 South Oak Street
Santa Ana, CA. 92707
Sales Office:
Tel. +1 (714) 960-5152 x204
Fax +1 (714) 960-2505
Factory:
Tel. +1 (714) 540-8454 x166
Fax. +1 (714) 540-1299
Email: [log in to unmask]
Web Site: www.thermalworks.com
----- Original Message -----
From: "Rick" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 21, 2002 4:24 AM
Subject: [TN] (Fwd) Inquiry on maximum temperature
> ------- Forwarded message follows -------
> Date sent: Mon, 20 May 2002 13:42:16 -0700
> From: Dino Accoto <[log in to unmask]>
> Subject: Inquiry on maximum temperature
>
> Dear Sir,
>
> I am working at the RPL lab - Stanford University, on a project
> aimed at the fabrication of a microvalve. One of the possible
> technologies to fabricate the body of the valve is PCB. Is there any
> available data about which maximum temperature a PCB can operate at for
> a long time so that no appreciable deformation/material damage occur?
>
> Thanks in advance for your information,
> Dino Accoto
>
>
>
>
> Rick Babyak
> Process Engineer
> Proto Circuit Inc.
> 7 Ascot Parkway
> Cuyahoga Falls, OH 44223
> 330-572-3400
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|