TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vwZTo-0000p8C; Mon, 17 Feb 97 14:16 CST
Encoding:
38 Text
Old-Return-Path:
Date:
Mon, 17 Feb 97 14:03:45 cst
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10321
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"QjsZo3.0.z0F.3oB2p"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
From [log in to unmask] Tue Feb 18 13:
06:47 1997
Message-Id:
Parts/Attachments:
text/plain (51 lines)
     Hi Greg -
     
     We have used the Kleenox material off and on depending on the process 
     situation. We have never had an issue with it except for the really 
     wonderful odor that is generated as it does its job. It doesn't take 
     very much Kleenox to de-dross the pot - are you using too much thus 
     ending up with buildup or maybe you are having a Kleenox/flux 
     reaction.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]
     


______________________________ Reply Separator _________________________________
Subject: Dross reducer (Kleenox)
Author:  [log in to unmask] at ccmgw1
Date:    2/15/97 12:04 AM


Does anyone out there in Flow Solder land use Kleenox dross reducing agent 
and if so do you see any abnormal material on the sides of walls in the 
solder pot or built up on the splash plates of the chip and lambda waves.
     
gregory.....
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2