Hi Greg - We have used the Kleenox material off and on depending on the process situation. We have never had an issue with it except for the really wonderful odor that is generated as it does its job. It doesn't take very much Kleenox to de-dross the pot - are you using too much thus ending up with buildup or maybe you are having a Kleenox/flux reaction. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Dross reducer (Kleenox) Author: [log in to unmask] at ccmgw1 Date: 2/15/97 12:04 AM Does anyone out there in Flow Solder land use Kleenox dross reducing agent and if so do you see any abnormal material on the sides of walls in the solder pot or built up on the splash plates of the chip and lambda waves. gregory..... *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************