One thought is to make them much more brittle by holding at liquid
nitrogen temperature during machining. They would probably behave like
a metal. Perhaps laser cutting is a possibility. Or oxygen plasma etch
after your regular matching. These are just ideas, no experience.
Pat Hogue
Materials and Processes
[log in to unmask]
> ----------
> From: Torben Østeraa[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Torben Østeraa
> Sent: Sunday, June 07, 1998 3:14 AM
> To: [log in to unmask]
> Subject: [TN] Machining of polyimide flex material.
>
> Dear collegues,
>
> We are a producer of R/F pwb's. The great majority of jobs run in very
> small numbers, so we have to avoid expensive tooling. As a
> consequence,
> all machining of part-components and finished panels is done by
> nc-routing.
> Unfortunately, we have been unable to avoid burring of the quite tough
> polyimide laminate. Therefor, a substantial work is put into manual
> 'deburring'.
> This is a very time consuming operation which we would like to avoid.
> Any
> advise regarding optiming routing or experinces with possible
> alternaive
> methodes, e.g. water-jet or laser cutting, would be very welcome.
>
> Regards
>
> Torben Oesteraa
> [log in to unmask]
> Printca AS
> Denmark
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|