Dear collegues,
We are a producer of R/F pwb's. The great majority of jobs run in very
small numbers, so we have to avoid expensive tooling. As a consequence,
all machining of part-components and finished panels is done by nc-routing.
Unfortunately, we have been unable to avoid burring of the quite tough
polyimide laminate. Therefor, a substantial work is put into manual
'deburring'.
This is a very time consuming operation which we would like to avoid. Any
advise regarding optiming routing or experinces with possible alternaive
methodes, e.g. water-jet or laser cutting, would be very welcome.
Regards
Torben Oesteraa
[log in to unmask]
Printca AS
Denmark
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|