TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Barmuta, Mike" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Barmuta, Mike
Date:
Fri, 12 Nov 2004 15:16:42 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (56 lines)
Hi Glynn: I not exactly sure what you are referring to as "switches" and
"wiping actions". If you are talking about rotary switches and wiper cycles,
immersion Au will never come close to 250,000 cycles.
Electroplated hard acid Au will give you 100,000+ cycles at 20-30 u".
However a lot depends on the wiper/contact design, pressure and material of
construction. Key pad switches are good for over 1,000,000 using the same
type of plating and thickness.


                                                        Regards

Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076
-----Original Message-----
From: Glynn Shaw [mailto:[log in to unmask]]
Sent: Friday, November 12, 2004 8:00 AM
To: [log in to unmask]
Subject: [TN] ENIG as edge-connector finish


I thought I read somewhere that IPC said Enig was an acceptable finish for
switches and would withstand in excess of 250,000 wiping actions. Does
anyone know if 150 micro inches electroless nickel with 4-6 micro inches
immersion gold is acceptable as a finish for edge connectors?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2