TECHNET Archives

November 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 9 Nov 2012 10:02:27 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Julie Silk <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (40 lines)
I'd say "cottage" fix up.  {shudder}

__________
Julie Silk 
Environmental Compliance Technical Program Manager
EMG Customer Experience and Quality
Agilent Technologies, Inc
[log in to unmask]
707-577-4296 (TN 577-4296)


-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]] 
Sent: Friday, November 09, 2012 8:11 AM
To: 'TechNet E-Mail Forum'; SILK,JULIE (A-Sonoma,ex1)
Subject: RE: [TN] Limits on flux residue

"the practice of injecting flux and reheating to hope that the bad joints melt together." Is it industry approved method (I mean with published reliability data to compare with non-repaired part)?  Or just "cottage" fix up method (anything goes, as long as make it work for the moment, like wet towel wrap of a heat up unit for example)?   

Joyce Koo
Materials Researcher - Materials Interconnect Lab Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk
Sent: Friday, November 09, 2012 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] Limits on flux residue

Are the open joints caused by the excessive flux?  Or are both the excessive flux and the open joints caused by rework?  I would bet on the latter.  I can't visualize a scenario where the flux would cause good joints to open.  Ugly, sure, but very common with reworked BGAs.  Reworking BGAs does not always successfully make good joints on all balls, and neither does the practice of injecting flux and reheating to hope that the bad joints melt together.  It's possible and even likely that they make a contact joint vs metallurgical that fails later.  The flux is a symptom, not a cause.

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2