I'd say "cottage" fix up. {shudder} __________ Julie Silk Environmental Compliance Technical Program Manager EMG Customer Experience and Quality Agilent Technologies, Inc [log in to unmask] 707-577-4296 (TN 577-4296) -----Original Message----- From: Joyce Koo [mailto:[log in to unmask]] Sent: Friday, November 09, 2012 8:11 AM To: 'TechNet E-Mail Forum'; SILK,JULIE (A-Sonoma,ex1) Subject: RE: [TN] Limits on flux residue "the practice of injecting flux and reheating to hope that the bad joints melt together." Is it industry approved method (I mean with published reliability data to compare with non-repaired part)? Or just "cottage" fix up method (anything goes, as long as make it work for the moment, like wet towel wrap of a heat up unit for example)? Joyce Koo Materials Researcher - Materials Interconnect Lab Research In Motion Limited Office: (519) 888-7465 79945 Mobile: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk Sent: Friday, November 09, 2012 10:59 AM To: [log in to unmask] Subject: Re: [TN] Limits on flux residue Are the open joints caused by the excessive flux? Or are both the excessive flux and the open joints caused by rework? I would bet on the latter. I can't visualize a scenario where the flux would cause good joints to open. Ugly, sure, but very common with reworked BGAs. Reworking BGAs does not always successfully make good joints on all balls, and neither does the practice of injecting flux and reheating to hope that the bad joints melt together. It's possible and even likely that they make a contact joint vs metallurgical that fails later. The flux is a symptom, not a cause. --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________