Kevin,
Make sure you require a Ni barrier layer between the copper and gold (hard
of soft)!
Chuck
Charles W. Brummer | 3M Manufacturing Engineer
3M Electronic Solutions Division
3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com
This message (including any attachments) may contain material, non-public
information or proprietary information and is for the intended recipients
only. If you are not the intended recipient, you should notify the sender
and delete this message. Any disclosure, copying, or use of this
information is strictly prohibited and may subject you to legal liability.
From: "Glidden, Kevin" <[log in to unmask]>
To: <[log in to unmask]>
Date: 08/14/2012 09:15 AM
Subject: [TN] PCB finish: ENIG vs. hard gold
Sent by: TechNet <[log in to unmask]>
Hi everyone,
We have a PCB supplier who is offering "Hard Gold" as an alternate to ENIG
finish, due to PCB size and processing capabilities. The application is
Class 3 (mil/aero). The circuit is thin FR4 and subject to SMT reflow w/
Sn63Pb37 (non RoHS) solder alloy, and moderate flexing in end application.
Can anyone offer info on the differences between the two finishes, and/or
their suitability? Is there an IPC spec (or specs) that outline "hard
gold"?
Thanks,
Kevin Glidden
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|