We see these all the time, the parts are not stable since the leads are not
planar to the part so the diodes rock. The lead goes under the part and
takes the solder there as well giving you not much wicking up the lead. We
have pickup misses as well from the feeders since the parts tend to tip in
the pockets. But not a defect.
Dave Chapman
Manufacturing Engineer
Circuit Service Inc.
-----Original Message-----
From: Lance Mayes [mailto:[log in to unmask]]
Sent: Tuesday, September 02, 2003 2:16 PM
To: [log in to unmask]
Subject: [TN] pic's
Importance: High
I have attached some pictures of components that always seem to have one
joint that is not soldered as the other end. These happed mainly with this
component at various sites on the board. Is this a contamination a
disturbed joint or a cold joint. This is an SMT process and the problems
vary
on the runs. I would like to know if this is a defect for class 2 or not.
Thanks in advance for your time.
P. Lance Mayes
Mfg. Trainer
----- Forwarded by Lance Mayes/CO-GRA/Ametek on 09/02/03 01:07 PM -----
Howard Watson
08/27/03 05:33 PM
To: Lance Mayes/CO-GRA/Ametek@Ametek
cc:
Subject: pic's
Howard Watson
SMT Manufacturing Engineer
AMETEK/Dixson
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|