Hi Rich - get a copy of the following: "The Effect of Gold on the
Reliability of Fine Pitch Surface Mount Solder Joints" , authors
Glazer,Kramer, Morris Jr., Circuit World, vol 18, No. 4, 1992, pages 41-46.
It contains the information you are looking for. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Richard G. Wenda" <[log in to unmask]> on 02/18/99 12:39:00 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
To: [log in to unmask]
cc:
Subject: [TN] gold embrittlement
Dear TN,
I am looking for a white paper or perhaps an article on the effects of
gold volume to solder reflow reliability. Apparently NCMS had an
article in ~spring of '96, co-authored by Wenger and Janus,
determining that 3% was an allowable percentage.
If you know how I can find this paper I would appreciate it. If you
know of more recent studies that might help as well.
Thank you, Rich.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|