TECHNET Archives

February 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
David D Hillman <[log in to unmask]>
Date:
Thu, 18 Feb 1999 21:05:40 -0600
Content-Type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David D Hillman <[log in to unmask]>
Parts/Attachments:
text/plain (63 lines)
Hi Rich - get a copy of the following: "The Effect of Gold on the
Reliability of Fine Pitch Surface Mount Solder Joints" , authors
Glazer,Kramer, Morris Jr., Circuit World, vol 18, No. 4, 1992, pages 41-46.
It contains the information you are looking for. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]





"Richard G. Wenda" <[log in to unmask]> on 02/18/99 12:39:00 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to [log in to unmask]

To:   [log in to unmask]
cc:
Subject:  [TN] gold embrittlement




     Dear TN,

     I am looking for a white paper or perhaps an article on the effects of
     gold volume to solder reflow reliability.  Apparently NCMS had an
     article in ~spring of '96, co-authored by Wenger and Janus,
     determining that 3% was an allowable percentage.

     If you know how I can find this paper I would appreciate it.  If you
     know of more recent studies that might help as well.

     Thank you, Rich.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2