TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Darrel Therriault <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 13 Feb 2001 09:36:50 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
Spencer,

We have used Entek 106A with good success from a solderability standpoint.
The problems we encountered were :

1.      ICT probes tend to get "gummed" up frequently from the OSP. We fixed
this problem by
        adding all TPs to the solder stencil so we had a solder contact
surface.

2.      Some of our boards require large grounding surfaces and the OSP does
not make for a good
        conductive coating or it gets washed away and the copper then
oxidizes and contact is
        not acceptable.

These were reason enough to change to a metal finish.

DT





-----Original Message-----
From: Spencer Davis [mailto:[log in to unmask]]
Sent: Tuesday, February 13, 2001 6:48 AM
To: [log in to unmask]
Subject: [TN] Entek OSP


What are the fabrication, assembly and test issues associated with Entek OSP
vs other finishes.  We want to use it for double sided surface mount
assemblies.

Spencer Davis
Sr. Manufacturing Engineer
Spinnaker Networks, Inc.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2