> Timothy,
> I layed out a few designs that have wave soldered IC's.  I disagree
with Jan on 
> the orientation of the IC as it enters the wave.  Since ascii graphics
is not my
>  forte I will explain using his picture as an example.  First turn the
IC 90 Deg
> .  At the trailing end of the IC add "robber pads".  These are a set
of extra pa
> ds following the last pads on the IC.  Their purpose is to draw solder
off the l
> ast pins to keep them from bridging with their neighbors.  

Hi John,
I'm sorry, but i disagree with you on one thing. Of course if your'e
adding "robber pads" and rotate the ic 90 deg it sure work without
getting any bridging. 
But if you can't add any pads? Then i would do as i described using a
chip-wave, ofcourse, in a nitrogen wave solderer. I it find most logical
to run the ic with standard pads this way, then ofcourse i don't have
alot of experience in soldering smt with a wave solderer, but i've been
there.

Jan Merstrand 
Wave Soldering Technician

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2