     Marshall:
     
     Not to hedge, but it depends.  If you are in Arizona in the summer you 
     could probably leave it out for a week, but in Florida in the summer 1 
     hour could be to long.  It really depends on the ambient conditions.  
     To be on the safe side the rigid-flex should be baked 1 hr @ 250 F 
     prior to solder operation.  If you need to leave out for a period of 
     time after bake, leave parts under a heat lamp.
     
     Regards,
     
     Ron Yanuszewski


______________________________ Reply Separator _________________________________
Subject: Assy: Rigid Flex
Author:  [log in to unmask] at !INTERNET
Date:    1/24/97 2:00 AM


What is the maximum period of time that a rigid-flex board consisting of 
glass reinforced polyimide board and polyimide flex, can be left out of the 
dry box on the assembly floor before it should be re-baked to insure that it 
will not blister or de-laminate?
     
Thanks in advance for helping clear up a discussion between a board supplier 
and an assembler.
     
Marshall Andrews
[log in to unmask]
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2