We have a customer with this capability.
Lenthor Engineering
1506 Gladding Court
Milpitas, CA 95035
Tel: (408) 945-8787
Fax: (408) 945-0347
Contact: Jerry Smith
There are quite a few mil-spec shops that could do this for you.
Andrew P. Magee - Applications Engineer
Rogers - Circuit Materials Unit
Tel: (602) 917-5237
Fax: (602) 917-5256
E-Mail: 7403202@mcimail
______________________________ Reply Separator _________________________________
Subject: Rigid Flex Referral
Author: StephenJ (Steve Joy) {NAME:Steve
Joy|EMS:INTERNET|MBX:[log in to unmask] at MCIMAIL
Date: 9/7/95 1:21 PM
I am looking for a shop that is capable of building a rigid flex with the
following criteria: 10 layers/L4-5 flex; .003/.003" on the flex;
005/.005" on the epoxy; ~2000 holes- mostly .0135"; about 9" X 14" with
3 flex legs off the main board.