How many are missing now? I have worked with some boards that were abused in
the manner you described and the pads that were still on the board were very
weak. I know this because some of the remaining pad pulled off when I lifted
the kevlar tape that is part of the thermo-bond process.
Would the remaining pads pass the tape pull test for solder mask adhesion?
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Francis Sun
> Sent: Wednesday, May 08, 2002 4:38 PM
> To: [log in to unmask]
> Subject: Re: [TN] Guidelines or standards for number of missing unused
> BGA pads allowed
>
>
> Mr. Moon,
>
> Thanks for your interest in my problem.
> It is unfortunate, but we are relatively new with BGAs,
> and our rework personnel and Engineers are/were not familiar
> with the procedures to reduce heat and be gentle when cleaning the solder
> from the pads.
> Live and learn.
>
> Hope you or anyone out there can help.
>
>
> Regards;
>
> Frank Sun
> IVHS
> (905) 624-3025 ext. 1235
> Fax: (905) 624-4572
>
>
> |---------+---------------------------->
> | | Earl Moon |
> | | <[log in to unmask]
> | | M> |
> | | |
> | | 05/08/2002 01:41 |
> | | PM |
> | | |
> |---------+---------------------------->
>
> >-----------------------------------------------------------------
> -------------------------------------------------------------|
> |
> |
> | To: [log in to unmask], Francis Sun
> <[log in to unmask]> |
> | cc:
> |
> | Subject: Re: Guidelines or standards for number of
> missing unused BGA pads allowed |
>
> >-----------------------------------------------------------------
> -------------------------------------------------------------|
>
>
>
>
> I'm missing something here? I've never lost a pad during thousands of
> rework/repair oparations.
>
> No disrespect. I just don't get it but am sure you will explain.
>
> MoonMan
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|