TECHNET Archives

February 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Date:
Wed, 2 Feb 2005 09:20:56 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
         Hi Ingemar:
                        Do you want to see a board that the coating has potato chipped?  I do not have anyone at the moment, but it is easy to do.  Get a scrap board that is coated with polyurethane or Acrylic, soak it in alcohol for about five minutes. Place the soaked board in a sealed container. Leave it there 24 hours or so.  The board coating will be very soft and in some areas will look like potato chips.
        Regards,
        Ramon


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Wednesday, February 02, 2005 3:17 AM
To: [log in to unmask]
Subject: Re: [TN] Coating


Sure? That was a very frightening message! Do you have example? Can you send pic offline?
We've made a lot of boards for various aircrafts, with acrylic, never seen or heard of what you say.

Acrylic coating does not always withstand stillstanding contaminated water. Exposed a longer time to such
ionic wetness, the coating can absorb water, swell, and lift from the board. We don't know exactly how this
happens, and have just seen a few cases. Acrylic coating use to be splendid.
Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]
Sent: den 1 februari 2005 18:30
To: [log in to unmask]
Subject: [TN] Coating







  All Technetters :

 In advance, thanks for your insights.   Does anybody have any experience  with boards that are acrylic coated and exposed to Jet fuel fumes.?    Boards are not located next to the jets, but the fumes propagate to the boards that are housed in a metal cabinet. My understanding is that jet fuel is similar to kerosene.  Through experimentation, I know that alcohol fumes that are inside a close container with the a board , can weaken acrylic and polyurethane coating and sometimes the coating will potato chip.

    Regards,
    Ramon


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2