TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Adam Seychell <[log in to unmask]>
Date:
Mon, 16 Apr 2007 17:52:38 +1000
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Adam Seychell <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Does anyone know if stainless steel 316 corrodes when exposed to 
alkaline ammonia chloride etchants ?  I have this diaphragm pump with 
internal stainless steel fasteners which are exposed to the etchant. The 
pump elastomers are EPDM and santoprene, and body material is glass 
filled polypropylene. I am wondering if the pump can be used for 
alkaline etchants.

For a test I placed some stainless steel in etchant at let standing for 
one week. There was no visible surface corrosion, nor any measurable 
mass loss. I know this doesn't tell me I can use the pump and expect it 
to last.


best regards,
Adam Seychell

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2