I am trying to get a basic understanding on the "semi additive" process.
From what I understand, the copper base foil begins at 5um, and circuit
traces are electroplated to a desired thickness. Unlike conventional
"pattern plating" , there is no metal etch resist, but instead the
entire panel is etched just enough to remove the 5um copper base copper,
leaving the relatively thicker traces still in tack.
My question is, what steps are involved in obtaining the 5um copper base ?
The thinnest copper cladding I can find is 18um (1/2oz) which suggests
to me people are deposited 5um of electroless copper on blank PCB
insulating material.
If this is the case then will any of the direct metalization systems be
usable ? Due to the plating propagation effect with direct metalization,
there would be excessive variations in copper thickness over the whole
panel.
The only alternative I can see is to take standard 18um copper clad and
carefully etch down to 5um. The resulting 5um copper clad laminate could
then be used with direct metalization systems, however hole walls will
not have a 5um base, and therefore the hole wall plating finishes up
being 5um thinner than traces.
regards,
Adam Seychell
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|