TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Wed, 5 Mar 2008 12:57:20 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (74 lines)
Hi Jack! Let me put a different spin on what your associate read - You 
should NEVER put anything in the bag containing a pwb with a ImAg surface 
finish unless you know that the "anything" will not outgas/contaminate the 
surface finish. We always specify silver saver paper which does a good job 
of keeping outgassing/stuff away from the pwb. Some humidity indicators 
and desiccant materials are safe to put in the bag - you just need to do 
the homework. If you really want to see a reaction, put a rubberband in 
the pwb bag - wonderful surface species evolve (sulfur creatures)!   Good 
Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Jack Olson <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
03/05/2008 10:53 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Jack Olson <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Immersion Silver and Desiccants






One of my associates read somewhere (on a datasheet) that
desiccants should NOT be packaged with immersion silver boards,
(and seems to be putting a huge significance on that discovery)

My response would be:
OK. take out the desiccants and put in humidity indicators.
case closed.

Is there something else I should know about this?

Jack (aka "the new guy")

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2