TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Mon, 21 Jul 2008 12:01:20 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (70 lines)
Pete,

I may be wrong, but I claim that there is no ENIG reference picture or 
pictures. ENIG can have many faces, large 'grain' clusters, small clusters, 
bright appearance and dull,  typical gold colored and more like copper 
color,  hard surface and rather soft one, super flat and like Rocky 
Mountains seen in a SEM....it all depends (TM).  There are some traps 
also...you can study a ENIG board sample in a SEM, look hard on it with a 
LOM, do EDAX and other advanced investigations and find everything looking 
'good', while, at the same time, the sample is impossible to solder at. And 
vice versa.  For a serious qualification, I recommend some of the programs 
used by anyone with this forum,  George Wenger,  Dave Hillman, Richard 
Stadem or similar experienced guy. Myself, I could send lots of 'ENIG 
pictures' but I'm afraid these wouldn't be enough for a qualification. If 
you really mean to make a good qualification job, you'd better sit down and 
mail to any of the mentioned gurkas...sorry..gurus.

Inge

PS. If noone supports you, I'll send something offline to you, but later 
when I'm at my office.


----- Original Message ----- 
From: "Pete Houwen" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, July 21, 2008 6:58 AM
Subject: [TN] looking for ENiG photos


Our purchasing group is trying to qualify a new low cost PCB vendor, and I
have some reservations.  I have been examining their sample boards, and 
while
one oif them shows a normal ENiG grain under 800x magnification, the other 
is
flat and dull.  I believe it might be just gold plating.  It's hard to tell 
from the
cross sectons they sent (those display their own set of concerns).  I'm 
trying
to find some images to compare these, but I'm having no luck.  Does anyone
know of a good site where I might find some ENiG and Gold images?

Thanks,

Pete

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2